    The structure of acrylonitrile-butadiene rubbers paramagnetic-probe study
    (Lviv Polytechnic Publishing House, 2013) Livanova, Nadezhda; Karpova, Svetlana; Zaikov, Gennady
    Chain microstructures and supramolecular structures of nitrile-butadiene rubbers are studied by ESR spectroscopy. On the temperature dependences of the rotational mobility (correlation time τc) of paramagnetic probe 2,2,6,6-tetramethylpiperidine-1-oxyl, relaxation transitions are observed. It is shown that there is a correlation between the Arrhenius parameters of rotational mobility of radical and the copolymer composition and that different brands of rubbers differ in microstructure and supramolecular structure. Методом ЕСР-спектроскопії досліджено мікроструктуру та надмолекулярну структуру бутадієн-нітрильних каучуків. На температурних залежностях обертової рухомості (часу кореляції (τc)парамагнітного зонду 2,2,6,6-трет.метилпіперидин-1-оксил спостерігаються релаксаційні переходи. Встановлено зв‘язок між арреніусовськими параметрами обертової рухомості радикала і складом кополімерів та показано, що різні марки каучуків відрізняються мікро- та надмолекулярною структурою.
  • Thumbnail Image
    Item
    The structure of polybutadienes and butadiene-acrylonitrile copolymers
    (Publishing House of Lviv Polytechnic National University, 2011) Livanova, Nadezhda; Karpova, Svetlana
    The paramagnetic probe method with the use of free radicals of different dimensions (2,2,6,6-tetramethyl-1-piperidinyloxy and 4-benzoate-2,2,6,6-tetramethyl 1-piperidinyloxy) has been employed to study the effect of the isomeric composition of butadiene units in polybutadienes and butadiene–acrylonitrile copolymers on the number and dimensions of ordered structures. The nature of density fluctuations and defective regions, that is, the regions in which the radicals are sorbed, has been ascertained. It has been shown that the ordered regions are composed of stereoregular chain fragments, while defective regions are enriched with butadiene isomers different from those present in prevailing amounts. Методом парамагнітного зонду з використанням радикалів різної величини (2,2,6,6-тетраметил-піперидин-1-оксилу і 4-бензоат-2,2,6.6-тетраметилпіперидин-1-оксилу) досліджено вплив ізомерного складу бутадієнових ланок у полібутадієнах і кополімерах бутадієну з акрилонітрилом на кількість та величину впорядкованих структур. Встановлено природу флуктуацій густини і дефектних областей, в яких сорбовані радикали. Показано, що впорядковані області утворені стереорегулярними ділянками ланцюгів, а дефектні - збагачені ізомерами бутадієну.